The wall section is mounted to a Fire FurnaceThe wall section is mounted to a Fire Furnace

Burn Test of SIPs Wall

The vertically loaded EPS SIP gypsum board faced wall section is mounted to a Fire Furnace where 100% of the wall face is subjected to fire flame.

Temperature at the wall surface is maintained at 1000 degrees celcius for 1 hour.

Thermocouple rods are used to insure flame front at 100% of the wall surface at temperatures equal to or greater than 1,000 degrees celcius.